Author Topic: Element Lines Missing  (Read 1638 times)

rieders.n

  • Student
  • *
  • Posts: 3
Element Lines Missing
« on: January 14, 2018, 04:11:56 pm »
[In DTSA-II] the element markers for certain transitions no longer display in the spectrum when selected?  See example for Sn below, the M-lines are not showing even though they have been selected.  Has anybody else had this problem?  Thank You.

« Last Edit: January 14, 2018, 04:53:18 pm by John Donovan »

rieders.n

  • Student
  • *
  • Posts: 3
Re: Element Lines Missing
« Reply #1 on: January 15, 2018, 01:22:52 pm »
This is a bug in the software, all of the transitions are displayed if you change the energy scale once and change it back to the desired scale.