Author Topic: Image acquisition mode during automated analyses  (Read 2013 times)

Malcolm Roberts

  • Professor
  • ****
  • Posts: 134
Image acquisition mode during automated analyses
« on: October 14, 2015, 06:47:51 PM »
Hi John
Currently automated image acquisition uses SE. I would like to get BS images instead. Where can this change be facilitated in Probewin.ini? If the default cannot be changed, how can I get PfEPMA to acquire BS images? I've not had much luck! I've had a look through the manual at the layout of probewin.ini, but cannot see anything obvious.
Cheers,
Malc.

John Donovan

  • Administrator
  • Emeritus
  • *****
  • Posts: 3304
  • Other duties as assigned...
    • Probe Software
Re: Image acquisition mode during automated analyses
« Reply #1 on: October 14, 2015, 07:57:11 PM »
Hi John
Currently automated image acquisition uses SE. I would like to get BS images instead. Where can this change be facilitated in Probewin.ini? If the default cannot be changed, how can I get PfEPMA to acquire BS images? I've not had much luck! I've had a look through the manual at the layout of probewin.ini, but cannot see anything obvious.
Cheers,
Malc.

You can select BSE image acquisition from the Imaging dialog.  So just acquire a BSE image manually and then close the Imaging window, and the default signal should be saved for the automated imaging.
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"