Author Topic: Masters and PhD Theses  (Read 2980 times)

John Donovan

  • Administrator
  • Emeritus
  • *****
  • Posts: 2572
  • Other duties as assigned...
    • Probe Software
Masters and PhD Theses
« on: May 24, 2017, 09:41:30 am »
This topic is reserved for posting (and discussion?) of EPMA related Masters and PhD theses by graduates.  I hope those whose theses were focused on EPMA measurement or technique will feel free to "call their own number" and post their thesis as a pdf or at least provide a link for us.  After all, you put a lot of work into your writing and that effort should be shared with us all!   :)

The forum has a 16 MB limit for attachments, but if your thesis is larger than that please contact me and I can temporarily increase the limit or as I mentioned, you can simply post a link to it.
john
« Last Edit: May 24, 2017, 11:23:31 am by John Donovan »
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

Philippe Pinard

  • Post Doc
  • ***
  • Posts: 21
Re: Masters and PhD Theses
« Reply #1 on: June 11, 2017, 09:30:11 am »
My PhD thesis from RWTH Aachen University under the supervision of Silvia Richter.

doi: http://dx.doi.org/10.18154/RWTH-2016-08543