Author Topic: Strategies for Improving Accuracy Using Trace Elements Standards  (Read 6473 times)

Karsten Goemann

  • Global Moderator
  • Professor
  • *****
  • Posts: 206
Re: Strategies for Improving Accuracy Using Trace Elements Standards
« Reply #30 on: November 12, 2019, 02:23:45 pm »
Sure, can't do it this week as I'm doing monazite geochronology.

Do you want P10 or Xe? Normal or large PET? Does that matter?

Probeman

  • Emeritus
  • *****
  • Posts: 2051
  • Never sleeps...
    • John Donovan
Re: Strategies for Improving Accuracy Using Trace Elements Standards
« Reply #31 on: November 12, 2019, 02:38:45 pm »
No worries on timing. Only when you get a chance.

Better try and replicate Ben and my measurements as much as you can so reduce the variables, so please try a large PET using P-10.

Just curious if it's a crystal distorsion artifact or something else.