StrataGEM tutorials
« on: March 28, 2017, 11:41:55 AM »
Hi,

here is a nice application note from Bruker that gives a mini tutorial on how to use StrataGEM with EDS data. Originally, I had a few questions that I wanted to post here but this just resolved them nicely. Maybe it is helpful to others.

Question though: Does anyone have a manual or any other tutorials?
Against the dark, a tall white fountain played.

Probeman

  • Emeritus
  • *****
  • Posts: 2842
  • Never sleeps...
    • John Donovan
Re: StrataGEM tutorials
« Reply #1 on: March 28, 2017, 12:06:06 PM »
This isn't a tutorial, but I attach a paper below as an example of how to deal with measured elements that are common to both the thin film and the substrate.

Normally when both the thin film and the substrate *do not* contain common elements, and both thickness and composition are unknown, we can utilize multiple accelerating voltages to allow the analytical iteration in STRATAGem to converge. That is to say, by utilizing multiple accelerating voltages, e.g., 10, 15 and 20 keV, on both our bulk standards and our thin film unknowns, we can determine both the thickness and composition of our thin films. Multiple beam energies are required because at a single beam energy one can find a range of inversely varying compositions-thicknesses that fit the k-ratios from a single beam energy measurement.

So, for the situation where one is measuring an element that is present in both the thin film *and* the substrate, e.g., Ni-Si on Si or say, Ge-Si on Si, and both the thickness and the composition of the thin film are unknown, one must constrain something or the STRATAGem software will not converge on a solution.

The paper attached below (remember to login to see attachments!), describes an approach we developed at Univ of Oregon for these types of samples.  Please consider that if we are measuring an element in a thin film that is also present in the substrate, we are essentially subtracting two very large numbers from each other to obtain a very small number!
john
The only stupid question is the one not asked!

Probeman

  • Emeritus
  • *****
  • Posts: 2842
  • Never sleeps...
    • John Donovan
Re: StrataGEM tutorials
« Reply #2 on: March 28, 2017, 04:21:57 PM »
I took a draft document that Julie Chouinard had started a few years ago for our students, and since Anette asked so nicely, I decided to add a bit more detail to it. So attached below is a short tutorial on using STRATAGem to process intensities from Probe for EPMA in STRATAGem for thin film corrections.

Please let me know if you have any questions- it could cetainly be improved a lot.
john
« Last Edit: March 28, 2017, 04:41:32 PM by Probeman »
The only stupid question is the one not asked!