« Reply #15 on: June 26, 2019, 04:59:11 am »
Here is a pdf of my presentation yesterday on quantitative x-ray mapping for WDS EPMA (see attached file below if you are logged in).
john
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

John Donovan

  • Administrator
  • Emeritus
  • *****
  • Posts: 2507
  • Other duties as assigned...
    • Probe Software
Re: CalcImage Quantitative X-ray Mapping Examples
« Reply #16 on: January 15, 2020, 11:01:43 am »
We recently upgraded from Golden Software's Surfer 15 to Surfer 17.

One can choose the 32 bit version or the 64 bit version to install. We choose the 64 bit version. Interestingly the default installation folder that the Surfer installer offers you is "Surfer" as opposed to previous versions which always appended the Surfer version number to the folder by default, e.g., "Surfer 11" or "Surfer 15". We left the default installation folder as "Surfer" and proceeded with the installation which went fine.

Then we launched CalcImage and opened some existing maps, the first in Cameca (cartesian) stage mode as seen here for this alloy quantitative map in elemental weight percent:



and next in JEOL (anti-cartesian) stage orientation as seen here in this Mt St. Helens feldspar in oxide weight percent:



Bottom line, it appears that the CalcImage presentation output scripting still all works in the latest version (17) of Golden Software's Surfer app.
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

John Donovan

  • Administrator
  • Emeritus
  • *****
  • Posts: 2507
  • Other duties as assigned...
    • Probe Software
Re: CalcImage Quantitative X-ray Mapping Examples
« Reply #17 on: January 22, 2020, 12:10:14 pm »
We did some additional testing using the latest Surfer 17 from Golden Software, checking that the interactive "slicing" features all still work and it looks like they work as expected.

Here for illustration, is a slice through a zircon showing the uranium distribution, first using traditional off-peak measurements:



And here is the same acquisition, but processed using the MAN background correction:



And you can see, the MAN processed data has better precision, and even more importantly for x-ray map acquisitions, acquiring this map would have taken only 1/2 the acquisition time, since one only needs to acquire an on-peak x-ray map when using MAN!
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

Probeman

  • Emeritus
  • *****
  • Posts: 1984
  • Never sleeps...
    • John Donovan
Re: CalcImage Quantitative X-ray Mapping Examples
« Reply #18 on: January 30, 2020, 09:03:23 am »
I promised our EPMA students I would post this quant x-ray map they produced last quarter (better late than never I guess!):





15 keV, 30 nA, 100 ms per pixel