Hi,
I've just started using PFE for carbon analysis instead of the Jeol software. It looks good, both the calibration curve option and using phi-rho-z option with a blank assignment to remove contamination. Plus the acquire standards again at end of run.
Just a couple of suggestions, with calibration curve would it be possible to add other curve fitting routines, or more particularly force a straight line?
Using blank assignment, what do you think of the idea of being able to add standards as blank correction sample assigments, for example in this case I've acquired a series of 0-1wt.% C in Steel standards and it be nice to use the 0 wt.% C as the blank correction when using phi-rho-z option. But mainly for testing - allowing comparison of the two methods for the data. I surpose once you found which worked best your'd only need to do one or the other