Hi. We installed PfEPMA in our lab last week and here are a few bugs or glitches that we have noticed. Has anyone else noticed these and are there any fixes available? I will attach screen shots to demonstrate each of the points mentioned below.
1. Text is truncated in some places and is illegible.
2. The "Display PHA, Peaking and Scan" window disappears at the bottom of my monitor so we cannot see what is at the bottom of the window. Furthermore, we cannot raise the window or shrink it in any way to allow us to see the bottom of the window.
3. PfEPMA displays Beam 1, Beam 2, Absorbed 1 and Absorbed 2 but we believe that it is not labelling these currents properly. One would think Beam 1 and Beam 2 refers to the current read at the Faraday cup before and after analysis, and ABSD 1 and 2 refers to the absorbed current before and after analysis. However, it actually appears to be that Beam 1 and ABSD 1 refer to the beam current with Faraday cup, and Beam 2 and ABSD 2 refer to the before and after absorbed current.
4. Error message pops up when using TDI when an element with a multipoint background is used, though it appears that TDI is in fact applied.