General EPMA > EPMA Standard Materials
Spinel standards
JohnF:
I am looking for a spinel (MgAl2O4) epma standard. Anyone have something to share?
Probeman:
--- Quote from: JohnF on January 02, 2015, 03:30:27 PM ---I am looking for a spinel (MgAl2O4) epma standard. Anyone have something to share?
--- End quote ---
Hi John,
I have a lot of this wollastonite:
http://probesoftware.com/smf/index.php?topic=222.msg997#msg997
Good for major silicon and aluminum.
JohnF:
I think you meant Si and Ca (no Al in wollastonite, CaSiO3)
John Donovan:
--- Quote from: JohnF on January 04, 2015, 03:25:09 PM ---I think you meant Si and Ca (no Al in wollastonite, CaSiO3)
--- End quote ---
Yes, sorry. I ain't no darn geologist!
But that does remind me: I'd love to find a super pure end member aluminum silicate, such as sillimanite.
Gseward:
JohnF and I discussed this off-line. We discovered this:
http://www.mtixtl.com/mgal2o4spinel.aspx