Author Topic: Empirical PHA setup procedure  (Read 822 times)

JohnF

  • Professor
  • ****
  • Posts: 105
  • CQ DX DE WA3BTA
    • John's EPMA
Empirical PHA setup procedure
« on: April 03, 2024, 07:30:01 PM »
Can someone post the procedure for creating the EMPPHA.DAT table? Is it created manually, or is there some module that does it for you? And if manually generated, what is the format of the table? Thanks.

Probeman

  • Emeritus
  • *****
  • Posts: 2860
  • Never sleeps...
    • John Donovan
Re: Empirical PHA setup procedure
« Reply #1 on: April 03, 2024, 09:35:18 PM »
The only stupid question is the one not asked!