Author Topic: quantification of thinfilms on substrate data sets  (Read 917 times)

rraman64

  • Student
  • *
  • Posts: 2
quantification of thinfilms on substrate data sets
« on: February 13, 2024, 09:56:39 AM »
Hi,
I hit on DTSA while working with XRF & EDX analysis for thinfilms on silicon substrate. Instantly got hooked due to the simplicity in simulations & analysis.

While simulation options support thinfilm on substrate configuration, quantification methods do not support thinfilm/substrate configurations. If we use the available quantification method, we have to assume that film and substrate as homogeneous mixture.
stripping Si is not satisfactory.

Is there any other method to handle thinfilms?

Also is there any option to go for standardless analysis using ZAF (similar to PYMCA for XRF)?

thanks
rajaraman
« Last Edit: February 13, 2024, 10:13:20 AM by John Donovan »

John Donovan

  • Administrator
  • Emeritus
  • *****
  • Posts: 3304
  • Other duties as assigned...
    • Probe Software
Re: quantification of thinfilms on substrate data sets
« Reply #1 on: February 13, 2024, 10:14:59 AM »
While simulation options support thinfilm on substrate configuration, quantification methods do not support thinfilm/substrate configurations. If we use the available quantification method, we have to assume that film and substrate as homogeneous mixture.
stripping Si is not satisfactory.

Is there any other method to handle thinfilms?

You might want to check out BadgerFilm which is also free and designed specifically for quantification of thin films on substrates:

https://probesoftware.com/smf/index.php?board=37.0
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

Nicholas Ritchie

  • Moderator
  • Professor
  • *****
  • Posts: 155
    • NIST DTSA-II
Re: quantification of thinfilms on substrate data sets
« Reply #2 on: February 13, 2024, 02:11:39 PM »
John's advice is good.  You can use DTSA-II to extract the k-ratios (via fitting to standards) which you then plug into BadgerFilm.
"Do what you can, with what you have, where you are"
  - Teddy Roosevelt

rraman64

  • Student
  • *
  • Posts: 2
Re: quantification of thinfilms on substrate data sets
« Reply #3 on: February 13, 2024, 07:57:51 PM »
Thanks a lot Prof Ritchie & Prof John for the prompt suggestions.
I will explore the Badgerfilm and get back!