Author Topic: quantification of bulk samples  (Read 278 times)

Ben Buse

  • Professor
  • ****
  • Posts: 488
quantification of bulk samples
« on: August 17, 2023, 07:02:21 AM »
Hi,

In terms of bulk analysis are there any batch capabilities for multiple datapoints, or do you envisage it to be a tool for checking whether improvements could be made over standard software routines, rather than applying it to a large dataset

Thanks

Ben

Probeman

  • Emeritus
  • *****
  • Posts: 2823
  • Never sleeps...
    • John Donovan
Re: quantification of bulk samples
« Reply #1 on: August 17, 2023, 10:07:54 PM »
Hi,

In terms of bulk analysis are there any batch capabilities for multiple datapoints, or do you envisage it to be a tool for checking whether improvements could be made over standard software routines, rather than applying it to a large dataset

Thanks

Ben

Note that you can reprocess any number of data points in CalcZAF using an input file:

https://probesoftware.com/smf/index.php?topic=1342.msg10390#msg10390
The only stupid question is the one not asked!