Hi,

How are the errors calculated for export to output format? When using average of datapoints for k-ratio what error is being exported?

is it standard deviation? is it count stats - and does that use assume multiple points homogeneous and treat as multiple points x time? i.e. standard error?

Thanks

Ben

Ben Buse

  • Professor
  • ****
  • Posts: 499
Re: Error calculation: Save StrataGem/Badgerfilm output Format
« Reply #1 on: July 04, 2024, 08:23:30 AM »
Ok it seems PFE does not export errors to badgerfilm/stratagem; with badgerfilm assigning a 5% error to each element

Would it be a good idea to export errors?

John Donovan

  • Administrator
  • Emeritus
  • *****
  • Posts: 3304
  • Other duties as assigned...
    • Probe Software
Re: Error calculation: Save StrataGem/Badgerfilm output Format
« Reply #2 on: July 04, 2024, 10:41:54 AM »
Ok it seems PFE does not export errors to badgerfilm/stratagem; with badgerfilm assigning a 5% error to each element

Would it be a good idea to export errors?

The STRATAGem format does not seem to support error values. I guess one could create a new field type but STRATAGem will never support it and it would be up to Aurelien to add this capability to BadgerFilm:



My take on users asking about errors in the thin film calculation is that at the very least one can simply propagate the relative variances display for the k-ratios in Probe for EPMA.  Here is a quick way to see the variances quickly in Probe for EPMA:



First click the Analyze! button, then click the KRaws button...  note the %REL SD output.