Hi,

I would like to model X-ray distribution and yield of inclined grain boundaries and/or exsolutions. From what I can see Casino 2 only allows me vertical grain boundaries and Casino 3D does not model X-rays. I feel like there may be a way in McX-ray by using a cylinder in a box but I am just not quite getting the geometry settings.

Does anyone have any insights, suggestions, recommendations? Thanks!
Against the dark, a tall white fountain played.

Nicholas Ritchie

  • Professor
  • ****
  • Posts: 155
    • NIST DTSA-II
Re: Modelling inclined grain boundaries or exsolutions?
« Reply #1 on: June 22, 2023, 05:41:22 AM »
With a little scripting, this can be done in DTSA-II.

I can help write the script if can describe the desired geometry a little more precisely.
"Do what you can, with what you have, where you are"
  - Teddy Roosevelt

Anette von der Handt

  • Global Moderator
  • Professor
  • *****
  • Posts: 355
    • UMN Probelab
Re: Modelling inclined grain boundaries or exsolutions?
« Reply #2 on: June 23, 2023, 11:56:15 AM »
Fantastic! I'll send you an email.
Against the dark, a tall white fountain played.

John Donovan

  • Administrator
  • Emeritus
  • *****
  • Posts: 3304
  • Other duties as assigned...
    • Probe Software
Re: Modelling inclined grain boundaries or exsolutions?
« Reply #3 on: June 23, 2023, 09:59:51 PM »
With a little scripting, this can be done in DTSA-II.

I can help write the script if can describe the desired geometry a little more precisely.