Author Topic: An Open Letter to the Microanalysis Community  (Read 806 times)

crystalgrower

  • Professor
  • ****
  • Posts: 59
Re: An Open Letter to the Microanalysis Community
« Reply #15 on: November 26, 2021, 02:11:10 PM »
FIRM WRITTEN price quotes are the first step.

Note added next day:  Also required would be the minimum order whether in kilos or $$$.

The "cost to synthesize" does not include the cost of raw materials.  Hf-free Zr will cost a lot more than natural Zr.  Then  there is the cost of making ZrO2 powder, then the recrystallizatio

ZrO2 is usually stabilized with Y2O3: better make sure your spec is precise.  You may not have an option if the transition from low symmetry to cubic is below the melting point.  Charles Taylor had natural ZrO2 with 0, 5%, 10%, 15% and 20% Y2O3.  Below 15% Y2O3 the pieces were crappy polycrystalline dust.   But who knows where all that got to?

One  reason to avoid LaB6, CeB6 etc is the extremely high melting point.  Materials are usually sintered--pressed in a furnace but not melted.   Commercial RSi2 is a mix of R rich and Si rich phases , each phase about 1 micron across.

 
« Last Edit: November 27, 2021, 09:59:05 AM by crystalgrower »

Probeman

  • Emeritus
  • *****
  • Posts: 2256
  • Never sleeps...
    • John Donovan
Re: An Open Letter to the Microanalysis Community
« Reply #16 on: November 27, 2021, 08:26:25 AM »
Excellent advice.

Would you be able to help us locate some high purity ZrO2? And also perhaps some single crystal borides?  We only need a few grams to start our initial testing of purity and stoichiometry. Later we will want quotations for 500 to 1000 grams.

If you know of specific sources we would love to hear from you. This is a crowd sourced project, if we don't do it, no one else will.

Please send any written quotes to Will Nachlas:

Will Nachlas
Weeks Hall for Geological Sciences
1215 West Dayton St
Madison WI 53706

Will Nachlas <nachlas@wisc.edu>

or add the quotation information to our Google spreadsheet:

https://docs.google.com/spreadsheets/d/19AeXvxIaP6qvChbE7cxK05B_6rkZSN14T-7ZJ7nkm8M/edit*gid=0

We need all the help we can get, thank-you!
« Last Edit: November 27, 2021, 10:43:26 AM by Probeman »
The only stupid question is the one not asked!

wonachlas

  • Global Moderator
  • Student
  • *****
  • Posts: 4
Re: An Open Letter to the Microanalysis Community
« Reply #17 on: December 01, 2021, 10:32:24 AM »
I have a lead on potential sources for ZrO2 and YAG (Y3Al5O12). Does anyone have experience with materials from the Shelby Gem Factory? They were a world renowned synthesizer of several gemstones and apparently invented a technique for synthesis of CZ (ZrO2) using the Czochralski method. The factory closed in 2019 and all of the remaining stock was sold in bulk. I met a local gem dealer who claims to have obtained “hundreds” of pounds of bulk gemstones from the owner when it closed. I purchased ~7 g pieces of colorless ZrO2 and YAG. I will mount and test them for crystallinity and trace impurities to evaluate if materials from the Shelby factory could be suitable for our purposes.

sem-geologist

  • Professor
  • ****
  • Posts: 122
Re: An Open Letter to the Microanalysis Community
« Reply #18 on: December 04, 2021, 05:33:45 AM »
One  reason to avoid LaB6, CeB6 etc is the extremely high melting point.  Materials are usually sintered--pressed in a furnace but not melted.   Commercial RSi2 is a mix of R rich and Si rich phases , each phase about 1 micron across.

The high melting point was actually my main Pros to propose these REEB6, as that would be outstandingly stable under the electron beam. However, after doing more research on hexaboron structure, I came to see a much bigger problem for this material to be considered as standards.
I was trying to understand what oxidation state Ce inside CeB6 would be presented (generally REEB6, with REE as +2/+3/+4 and B +3/-5, looks not straight forward to understand). The structure of REEB6 can be described as B cage (B octhahedras connected in cubic fashion providing cells in between for REE) with entrapped REE in formed cells. Ideally stochiometric LaB6 (deep violet) is then all cells are occupied. But there can be vacancies, some sources suggest that in some extreme cases it can be 1/4 of cells not occupied by REE. Generally, it is easy to get slightly out of stochiometry values, and it is not so straight forward to check how much vacancies are there, without relying on other methods. The LaB6 which I have in one of SPI sets, and which looks very clean and homogenos, is clearly out from ideal stochiometry/has vacancies (phew, I at last have an explanation why it would give so systematically slightly different result compared with LaPO4 as standard). So REE-hexaborons are out from considerations. (They would still be excellent beam-shape standards for low voltage EDS, but should not be used as primary standards)

Probeman

  • Emeritus
  • *****
  • Posts: 2256
  • Never sleeps...
    • John Donovan
Re: An Open Letter to the Microanalysis Community
« Reply #19 on: December 06, 2021, 11:36:06 AM »
...dead time calibrations are probably a major area of inaccuracy. Paul Carpenter has tried to point this out for decades. If anyone out there is still using the "default" dead time calibrations provided to them at the time their instrument was installed, I can promise them that they have large accuracy problems. These gas detectors age quite dramatically over time and one should be re-running these dead time calibrations every year to two at most for reasonable accuracy.  This issue has actually gotten worse over time as both Cameca and JEOL have migrated to larger and larger Bragg crystals with increasing geometric efficiency.

So unless you always run a 10 nA or less, here is a link to Paul Carpenter's dead time spreadsheet which is very nice for performing your own dead time constant calculations using any software:

https://probesoftware.com/smf/index.php?topic=1160.0

It should be emphasized that utilizing standards that are not exactly matrix matched, will result in accuracy errors if ones instrument is not properly calibrated. Paul Carpenter and John Fournelle and been consistently making this point for decades, and before them it was Dan Weill and John Armstrong...  when will we ever learn?

To make this point clearer, I am attaching an abstract and presentation by Paul and John (but not George and Ringo!), from about 15 years ago.

Unfortunately I don't think things have gotten any better on this front since then.  The good news is that the synthetic high accuracy high purity minerals that are being proposed in the topic will help reveal to what extent our instrument require proper re-calibration of detector dead times, PHA settings, effective takeoff, etc., etc.
« Last Edit: December 06, 2021, 01:14:35 PM by Probeman »
The only stupid question is the one not asked!

qEd

  • Professor
  • ****
  • Posts: 25
Re: An Open Letter to the Microanalysis Community
« Reply #20 on: December 06, 2021, 06:03:21 PM »
One possibility for evaluating the synthetic crystals for stoichiometry under consideration for this endeavor is X-ray synchrotron diffraction imaging. I have never performed such a measurement, but imagine there are a number of beam lines that could be used to determine the distribution of defects/inclusions in a multi-mm cm?-sized crystal to verify the structure on a spatially resolved basis. 

crystalgrower

  • Professor
  • ****
  • Posts: 59
Re: An Open Letter to the Microanalysis Community
« Reply #21 on: December 13, 2021, 12:51:53 PM »
I will not comment on the ZrO2 because it belongs in a separate topic.

There is absolutely no reason for individuals to go and get price quotes because they will not be valid for the body that would be making the purchase according to the plan in the first post. 

Individuals are NOT representatives of the money holding body for the purpose of signing contracts for custom syntheses or purchases.

In any case the price quotes will probably expire  before any formal agreement to spend funds will be reached.

Lab managers who purchase supplies and sometimes instruments should be familiar with the process of funds being approved.  I don;t know how any professional could get an idea that crowdsourcing tactics are going to collect  any valid information towards  a corporate purchase. 

And since you haven't been placing orders for custom materials, please be aware that a sample is not released  until a contract is signed.  A significant part of the total price is required to be paid before ANY work of synthesis begins.


Probeman

  • Emeritus
  • *****
  • Posts: 2256
  • Never sleeps...
    • John Donovan
Re: An Open Letter to the Microanalysis Community
« Reply #22 on: December 13, 2021, 04:30:48 PM »
I will not comment on the ZrO2 because it belongs in a separate topic.

There is absolutely no reason for individuals to go and get price quotes because they will not be valid for the body that would be making the purchase according to the plan in the first post. 

Individuals are NOT representatives of the money holding body for the purpose of signing contracts for custom syntheses or purchases.

In any case the price quotes will probably expire  before any formal agreement to spend funds will be reached.

Lab managers who purchase supplies and sometimes instruments should be familiar with the process of funds being approved.  I don;t know how any professional could get an idea that crowdsourcing tactics are going to collect  any valid information towards  a corporate purchase. 

And since you haven't been placing orders for custom materials, please be aware that a sample is not released  until a contract is signed.  A significant part of the total price is required to be paid before ANY work of synthesis begins.

I adamantly disagree. The vendor information, availability and (rough) pricing is still valuable information for eventual group purchases.  Remember, we need to purchase small amounts initially to test for purity and stoichiometry.

Even more to the point, we are asking our community to investigate *all* possible sources for these materials, not only commercial sources but also state/government laboratories that may be able to offer our community such materials for *free*.  If we do the leg work.  You can decide for yourself if you would like to join this effort (or not).  :)
« Last Edit: December 13, 2021, 04:35:28 PM by Probeman »
The only stupid question is the one not asked!

Probeman

  • Emeritus
  • *****
  • Posts: 2256
  • Never sleeps...
    • John Donovan
Re: An Open Letter to the Microanalysis Community
« Reply #23 on: December 16, 2021, 07:00:26 PM »
I am attaching below (login to see attachments) documents from the global synthetic microanalysis standard project (unofficial):

1. Action plan

These are just draft ideas for how to proceed with this project. Will Nachlas is already moving ahead on a number of these steps and I hope you will participate. Check with the protocols he has specified including making careful instrument calibrations prior to any measurements, especially dead time calibrations on your WDS spectrometers.

2. Resources

Possible resources for obtaining high purity synthetic minerals, though we need your help to find/locate more materials and obtain rough pricing.

3. George Rossman's personal synthetic crystal collection (Cal Tech).

This is a spreadsheet from George Rossman showing what synthetic minerals have been produced in the past, as a guide to what *might* be possible to produce on larger scales for use as global microanalysis standards.
« Last Edit: December 16, 2021, 07:02:02 PM by Probeman »
The only stupid question is the one not asked!

crystalgrower

  • Professor
  • ****
  • Posts: 59
Re: An Open Letter to the Microanalysis Community
« Reply #24 on: December 17, 2021, 11:41:22 AM »
Under the original heading of sourcing  high quality materials:
I  learned a very different way of business with ACS and Mineralogical Society of America.

US Professional associations can incorporate as nonprofits for  their educational activities.  I have not checked to see if either MAS or Microscopy  Society of America have done this.
The benefit of having approval from a nonprofit to solicit donations of materials is that you may be able to solicit a much larger donation in return for a tax receipt.  Which tax receipt can only be issued by the financial officer of the association and their 503(b) registration number must appear. 
In fact a custom synthesis will never be donated without  100% of fair market  value including the cost of starting materials becoming a tax benefit.

Good Biz 101 is  not difficult or obscure. 
I have a specific concern.  The drive to  lowball legitimate businesses started with the forum survey asking users what they would like to pay as opposed to teaching them what it costs to make specialty pure materials.  Now users are being asked to carry out fishing   expeditions.   Should many users  falsely state they represent the MAS then the blowback might be worse than just denial of funds. 

The real intent of this Open Letter may be  to acquire some piles of materials not able to be sold for other reasons.   A pitch to ask for business leftovers  should have been stated up front, rather than all the noise about money possibly  sitting in the bank accounts of nonprofits. 
FYI: all those  pieces that SPI advertises are owned by Astimex Standards registered in Canada (no US tax benefit for donation) and the physical location might be a problem.

Users had better think very carefully where lowlballing small industry might lead.  About 10  years ago I found a small US company with SBIR grand funds, whose business was hydrothermal-grown  crystals of pure and layered materials.  They did not hand out free samples when asked.  They would have been the ideal place to commission Pb-free replacements for RPO4 of R=La-Gd (since all crucible fluxed methods leave contamination).  That commission could then have been donated to the NMNH as Lynn Boatner did with the original TVA materials.  But they  closed sometime before 2017. 

Probeman

  • Emeritus
  • *****
  • Posts: 2256
  • Never sleeps...
    • John Donovan
Re: An Open Letter to the Microanalysis Community
« Reply #25 on: December 17, 2021, 12:51:28 PM »
The real intent of this Open Letter may be  to acquire some piles of materials not able to be sold for other reasons.   A pitch to ask for business leftovers  should have been stated up front, rather than all the noise about money possibly  sitting in the bank accounts of nonprofits. 

Asking for commercial quotations, seeking state/government sources, asking for "leftovers" and custom synthesis are all activities that can be pursued in parallel, they are not exclusive pursuits.

Nachlas et al. are currently writing grant proposals, and matching funds may be required from "money in bank accounts of non profits", though exactly how that will be leveraged is up to those society directors.