Author Topic: High and low backgrounds  (Read 101 times)

Ben Buse

  • Professor
  • ****
  • Posts: 415
High and low backgrounds
« on: December 17, 2019, 02:09:58 am »
Hi,

Is it possible to export the values for the high and low backgrounds separately

Thanks

Ben

Doug_Meier

  • Post Doc
  • ***
  • Posts: 14
Re: High and low backgrounds
« Reply #1 on: December 17, 2019, 06:42:41 am »
The custom NIST output does this. I don't know if any of the others do as well. Last I checked, there was no user-specified checkbox that does the equivalent, so I create two output files (NIST and user-specified) when I require that additional information.

Probeman

  • Emeritus
  • *****
  • Posts: 1984
  • Never sleeps...
    • John Donovan
Re: High and low backgrounds
« Reply #2 on: December 17, 2019, 08:01:00 am »
Hi,

Is it possible to export the values for the high and low backgrounds separately

Thanks

Ben

Hi Ben,
When you say "the values", I assume you mean the raw x-ray intensities?

If so, Doug is correct, the only output mode that outputs the raw background intensities is the NIST output format. The Haldor-Topsoe and the John Hanchar output formats do output the interpolated off-peak intensities and the net (P-B) intensities but not the raw intensities. 

Of course the raw off-peak intensities are also output to the log window in DebugMode.