We have modified a Cameca holder for JXA-8530F before:

https://probesoftware.com/smf/index.php?topic=930.msg7540#msg7540

Recently we designed and made a top-reference type replacement for JEOL 9-holder (LH9). It is made of aluminum and done by chromate conversing coating. The holder has the exactly same size and height with JEOL's LH9. So far we are very satisfied with the holder.
« Last Edit: May 16, 2019, 08:46:53 am by John Donovan »

Probeman

  • Emeritus
  • *****
  • Posts: 2020
  • Never sleeps...
    • John Donovan
Re: JEOL 9-holder (LH9) replacement (top-reference type)
« Reply #1 on: May 16, 2019, 08:51:05 am »
Hi Changkun,
Are these holders top referenced like the Cameca sample holders?

Are you saying that your lab can manufacture and sell these holder to other labs?
john
The only stupid question is the one not asked!

Changkun

  • Post Doc
  • ***
  • Posts: 20
Re: JEOL 9-holder (LH9) replacement (top-reference type)
« Reply #2 on: May 16, 2019, 04:04:16 pm »
Hi John,

Yes.

You may be able to order the top-reference holder. But the machine shop has no website so only contacting via e-mail is available.