Does anyone know of a way to have Thermo Pathfinder not use a default 200 eV cutoff value when triggered by Probe for EPMA? No matter what I do when I change the Low Energy Cutoff value in Pathfinder and save it once an analysis starts from PfE the 200 eV default cutoff is automatically selected.

Thanks,
DAve

SteveSeddio

  • Moderator
  • Post Doc
  • *****
  • Posts: 19
  • Setting the mood for microanalysis...
Re: Pathfinder 200 eV cutoff
« Reply #1 on: April 12, 2019, 11:53:14 am »
Hi Dave,

Maybe  you have done these things, but here are two ideas:
1. Before beginning the acquisition with PfE, acquire an EDS spectrum from Pathfinder with the desired low energy cutoff. Then use PfE to acquire.
2. Create a Pathfinder project that has acquired spectra with the desired low energy cutoff. Then create a new project in that project and acquire data with PfE.

Let me know if either of these options help.
-Steve
Your friendly, neighborhood, EPMA-minded EDS guy.
stephen.seddio@thermofisher.com

DavidAdams

  • Post Doc
  • ***
  • Posts: 24
Re: Pathfinder 200 eV cutoff
« Reply #2 on: April 15, 2019, 05:15:42 am »
Thanks Steve!

I'll give those things a try