Does anyone know of/have access to a good, well characterised tourmaline standard reference material?

Thanks!
Dave

Anette von der Handt

  • Global Moderator
  • Professor
  • *****
  • Posts: 240
    • UMN Probelab
Re: Tourmaline Standard/Reference Material
« Reply #1 on: April 12, 2019, 07:44:25 pm »
Hi Dave,

a set of tourmalines (dravite, elbaite, schorl) from the Harvard collection was characterized by Dyar et al. (2001) and Leeman et al. (2001).

It is available for sale from the International Association of Geoanalysts: (http://iageo.com/microanalytical-reference-materials/) either individually or as a set.

Full references:
References for light elements:
Dyar, M.D., Wiedenbeck, M., Robertson, D., Cross, L.R., Delaney, J.S., Ferguson, K., Francis, C.A., Grew, E.S., Guidotti, C.V., Hervig, R.L., Hughes, J.M., Husler, J., Leeman, W., McGuire, A.V., Rhede, D., Rothe, H., Paul, R.L., Richards, I., Yates, M. (2001) Reference minerals for microanalysis of light elements. Geostandards Newsletter, 25, 441-463.

Leeman, W.P., Tonarini, S. (2001) Boron isotopic analysis of proposed borosilicate mineral reference samples. Geostandards Newsletter, 25, 399-403.