Hi Jakub,
John Donovan here. I am responding as "probeman" since that is my academic login for the forum.

Here's an interesting thing. In the Probe for EPMA software there are two additional options for the interference correction. One, to perform the 1993 interference correction, but *without* a matrix correction for the interfering line to account for the differences between the unknown composition and the standard used for the interference correction calibration. And two, the original Gilfrich interference correction which only relies on a simple ratio of the intensities. As seen here:



The Pb La/As Ka interference is probably not the best example to try these options with, but let's just see what happens. So here is the PbSiO3 (alamosite) example from the previous post, using the 1993 correction, but without the matrix correction term for differences between the unknown composition and the standard used for the interference correction calibration:

St  386 Set   3 Alamosite (PbSiO3)
TakeOff = 40.0  KiloVolt = 20.0  Beam Current = 30.0  Beam Size =    0
(Magnification (analytical) =  40000),        Beam Mode = Analog  Spot
(Magnification (default) =      400, Magnification (imaging) =    800)
Image Shift (X,Y):                                         .00,    .00

Tsumeb, South West Africa
From Mineralogical Research, CA
(assumed stoichiometric)
Number of Data Lines:   3             Number of 'Good' Data Lines:   3
First/Last Date-Time: 05/25/2015 05:30:18 PM to 05/25/2015 05:35:33 PM
WARNING- Using Exponential Off-Peak correction for pb la
WARNING- Using Exponential Off-Peak correction for as ka

Average Total Oxygen:         .000     Average Total Weight%:   99.577
Average Calculated Oxygen:    .000     Average Atomic Number:   63.145
Average Excess Oxygen:        .000     Average Atomic Weight:   56.780
Average ZAF Iteration:        4.00     Average Quant Iterate:    14.33

St  386 Set   3 Alamosite (PbSiO3), Results in Elemental Weight Percents
 
ELEM:        S      Pb      As      Si       O
TYPE:     ANAL    ANAL    ANAL    SPEC    SPEC
BGDS:      LIN     EXP     EXP
TIME:    80.00   80.00   80.00     ---     ---
BEAM:    29.88   29.88   29.88     ---     ---

ELEM:        S      Pb      As      Si       O   SUM 
   321   -.014  73.892  -1.109   9.910  16.939  99.617
   322   -.012  73.692  -1.054   9.910  16.939  99.475
   323   -.004  73.640   -.845   9.910  16.939  99.640

AVER:    -.010  73.741  -1.003   9.910  16.939  99.577
SDEV:     .006    .133    .140    .000    .000    .090
SERR:     .003    .077    .081    .000    .000
%RSD:   -56.98     .18  -13.93     .00     .00

PUBL:     n.a.  73.151    n.a.   9.910  16.939 100.000
%VAR:      ---     .81     ---     .00     .00
DIFF:      ---    .590     ---    .000    .000
STDS:      730     731     662     ---     ---

STKF:    .4736   .8044   .4976     ---     ---
STCT:   232.38  301.58   92.02     ---     ---

UNKF:   -.0001   .6275  -.0107     ---     ---
UNCT:     -.04  235.26   -1.97     ---     ---
UNBG:      .60   14.64    3.37     ---     ---

ZCOR:   1.1646  1.1752   .9398     ---     ---
KRAW:   -.0002   .7801  -.0214     ---     ---
PKBG:      .93   17.07     .41     ---     ---
INT%:     ----    ---- -104.55     ---     ---

It's actually somewhat better than with the matrix correction term! Again I suspect this is because the interference from the Pb La line on As relative to the Pb interference standard (galena), is not properly captured by the matrix correction term for As Ka.

And here is the sample again, but using the old Gilfrich interference correction:

St  386 Set   3 Alamosite (PbSiO3)
TakeOff = 40.0  KiloVolt = 20.0  Beam Current = 30.0  Beam Size =    0
(Magnification (analytical) =  40000),        Beam Mode = Analog  Spot
(Magnification (default) =      400, Magnification (imaging) =    800)
Image Shift (X,Y):                                         .00,    .00

Tsumeb, South West Africa
From Mineralogical Research, CA
(assumed stoichiometric)
Number of Data Lines:   3             Number of 'Good' Data Lines:   3
First/Last Date-Time: 05/25/2015 05:30:18 PM to 05/25/2015 05:35:33 PM
WARNING- Using Exponential Off-Peak correction for pb la
WARNING- Using Exponential Off-Peak correction for as ka

Average Total Oxygen:         .000     Average Total Weight%:   52.147
Average Calculated Oxygen:    .000     Average Atomic Number:   44.055
Average Excess Oxygen:        .000     Average Atomic Weight:   33.809
Average ZAF Iteration:        4.00     Average Quant Iterate:     2.00

St  386 Set   3 Alamosite (PbSiO3), Results in Elemental Weight Percents
 
ELEM:        S      Pb      As      Si       O
TYPE:     ANAL    ANAL    ANAL    SPEC    SPEC
BGDS:      LIN     EXP     EXP
TIME:    80.00   80.00   80.00     ---     ---
BEAM:    29.88   29.88   29.88     ---     ---

ELEM:        S      Pb      As      Si       O   SUM 
   321   -.015  24.574    .936   9.910  16.939  52.344
   322   -.013  24.358   1.003   9.910  16.939  52.196
   323   -.004  23.808   1.249   9.910  16.939  51.901

AVER:    -.011  24.247   1.062   9.910  16.939  52.147
SDEV:     .006    .395    .165    .000    .000    .225
SERR:     .004    .228    .095    .000    .000
%RSD:   -56.90    1.63   15.51     .00     .00

PUBL:     n.a.  73.151    n.a.   9.910  16.939 100.000
%VAR:      ---  -66.85     ---     .00     .00
DIFF:      --- -48.904     ---    .000    .000
STDS:      730     731     662     ---     ---

STKF:    .4736   .8044   .4976     ---     ---
STCT:   232.38  301.58   92.02     ---     ---

UNKF:   -.0001   .1797   .0099     ---     ---
UNCT:     -.04   67.36    1.84     ---     ---
UNBG:      .60   14.64    3.37     ---     ---

ZCOR:   1.2615  1.3495  1.0698     ---     ---
KRAW:   -.0002   .2234   .0200     ---     ---
PKBG:      .93    5.60    1.54     ---     ---
INT%:     ----  -71.37  -95.77     ---     ---

Not very good at all!  And in fact since the Gilfrich method was not iterated in its original implementation, it's doing better than it would have traditionally!

So the 1993 method is a definite improvement over Gilfrich as shown in the 1993 paper, but it could still be improved further as I hope you will be able to show, by utilizing the correct matrix correction term for the specific interfering line. 

One question that occurs to me is that how will you deal with a situation where more than one interfering line interferes with a specific analytical line.  Often we see a situation where several lines of different Bragg orders are involved in the interference.  The world is complicated!   :)