EPMA Software Designed By Users For Users
Welcome,
Guest
. Please
login
or
register
.
1 Hour
1 Day
1 Week
1 Month
Forever
Login with username, password and session length
News:
We are a community of analysts, that cares about EPMA
Home
Help
Search
Login
Register
Probe Software Users Forum
»
General EPMA
»
EPMA Sample Preparation
»
sputter coater plasma colour
« previous
next »
Print
Pages: [
1
]
Author
Topic: sputter coater plasma colour (Read 3501 times)
Ben Buse
Professor
Posts: 499
sputter coater plasma colour
«
on:
March 23, 2017, 08:40:30 AM »
Hi,
Does anyone know why on a gold sputter coater - the plasma changes from blue to pink during the sputtering? Is this normal?
Thanks
Ben
Logged
Ben Buse
Professor
Posts: 499
sputter coater plasma colour
«
Reply #1 on:
March 23, 2017, 08:42:27 AM »
Hi,
Does anyone know why the plasma changes from blue to pink during sputtering - on a gold sputter coater. Is this normal?
Thanks
Ben