Author Topic: Problem with Optical Monitor  (Read 3388 times)

Probeman

  • Emeritus
  • *****
  • Posts: 2856
  • Never sleeps...
    • John Donovan
Problem with Optical Monitor
« on: December 19, 2016, 04:51:30 PM »
All,
After bringing up the SX100 today after a chiller problem, everything seems to work fine except that there is no display of the optical image on the dedicated monitor.  The optical image displays just fine in the Cameca PeakSight software so the light and camera are fine. And if I cycle the power on the dedicated monitor, I see the optical image for a second or so, but then it goes black again.

I seem to remember this issue before, but I can't remember what the solution was...   any suggestions?
john
The only stupid question is the one not asked!

Probeman

  • Emeritus
  • *****
  • Posts: 2856
  • Never sleeps...
    • John Donovan
Re: Problem with Optical Monitor
« Reply #1 on: December 20, 2016, 12:25:16 PM »
All,
After bringing up the SX100 today after a chiller problem, everything seems to work fine except that there is no display of the optical image on the dedicated monitor.  The optical image displays just fine in the Cameca PeakSight software so the light and camera are fine. And if I cycle the power on the dedicated monitor, I see the optical image for a second or so, but then it goes black again.

I seem to remember this issue before, but I can't remember what the solution was...   any suggestions?
john

Seems to be a bad monitor, we replaced it and it's working again.
john
The only stupid question is the one not asked!