Author Topic: Alternatives to nitrile gloves  (Read 591 times)

dawncruth

  • Professor
  • ****
  • Posts: 76
Alternatives to nitrile gloves
« on: August 05, 2021, 10:10:12 PM »
During the height of the pandemic, I had a hard time getting M-sized gloves. This circumstance coupled with the single use nature of gloves got me wondering about more sustainable alternatives to nitrile gloves. JEOL ships cloth gloves with their probes. I assume these would be acceptable for sample changes and day to day activities. I would keep nitrile gloves on hand for other purposes, of course. But do we really need them for sample changes?

Nicholas Ritchie

  • Professor
  • ****
  • Posts: 155
    • NIST DTSA-II
Re: Alternatives to nitrile gloves
« Reply #1 on: August 06, 2021, 06:24:35 AM »
Many years ago, when I worked in ultra-high vacuum (~10^-10 Torr), we used nylon cloth gloves.  They provide less feel but are good at eliminating finger oils and other contaminants.   I'm not sure where we got them but I found something similar here: https://www.economic.com/cleanroom-supplies/cleanroom-gloves/nylon.html
"Do what you can, with what you have, where you are"
  - Teddy Roosevelt

Probeman

  • Emeritus
  • *****
  • Posts: 2858
  • Never sleeps...
    • John Donovan
Re: Alternatives to nitrile gloves
« Reply #2 on: August 06, 2021, 07:56:24 AM »
JEOL ships cloth gloves with their probes. I assume these would be acceptable for sample changes and day to day activities. I would keep nitrile gloves on hand for other purposes, of course. But do we really need them for sample changes?

Great question.  I think it all depends on the person.

Many years ago when I was taking a class in vacuum technology at Lawrence Berkeley Lab, the instructor had us each place a fingerprint on separate glass slides and then placed them one at a time in a vacuum chamber and used a residual gas analyzer (RGA) to look at the volatiles.

Most of my classmates had sky high readings from their fingers, but I was told I was born to be a vacuum technician because my fingers were "bone dry".  ;D

But in any case I think cloth gloves should be fine for changing EPMA samples, especially since the microprobe isn't technically an ultra high vacuum instrument.