Author Topic: Ultra Pure TiO2?  (Read 5890 times)

Probeman

  • Emeritus
  • *****
  • Posts: 2874
  • Never sleeps...
    • John Donovan
Ultra Pure TiO2?
« on: February 05, 2014, 02:47:08 PM »
Does anyone have a very pure TiO2 crystal or glass with ICP-MS or other trace characterization?

We want to test it as a suitable "blank" standard for rutile/anatase trace element analyses.
« Last Edit: February 10, 2014, 02:46:40 PM by John Donovan »
The only stupid question is the one not asked!

Jeremy Wykes

  • Professor
  • ****
  • Posts: 42
Re: Ultra Pure TiO2?
« Reply #1 on: February 05, 2014, 10:20:31 PM »
I suspect these might be quite pure:
http://www.mtixtl.com/tio2substrates.aspx

Edit by John: Thanks! We will check them out.
« Last Edit: February 10, 2014, 02:46:57 PM by John Donovan »
Australian Synchrotron - XAS

Karsten Goemann

  • Global Moderator
  • Professor
  • *****
  • Posts: 228
Re: Synthetic Quartz Standard?
« Reply #2 on: February 07, 2014, 04:11:22 PM »
We bought some synthetic rutile from P&H developments in the UK recently which is 99.999%, single phase. We have mounted it and, although we've not tested it thoroughly yet, it is looking good so far.

Malcolm Roberts

  • Professor
  • ****
  • Posts: 134
Re: Ultra Pure TiO2?
« Reply #3 on: February 10, 2014, 04:22:10 PM »
So messrs Plant and Hopkins are still producing standards. That is good to know. I thought they had retired......

Richard Walshaw

  • Post Doc
  • ***
  • Posts: 19
Re: Ultra Pure TiO2?
« Reply #4 on: March 14, 2014, 08:03:52 AM »
Tim Hopkins pops in here to use our SEM occasionally. I think he is now on his second retirement. He seems to spend most of his time in the Alps and just makes up a few standard blocks now and again to help fund his playboy lifestyle. He's got the right idea!
"Stay out of the black and in the red...there's nothing in this game for two in a bed." - Albert Einstein

Richard Walshaw

  • Post Doc
  • ***
  • Posts: 19
Re: Ultra Pure TiO2?
« Reply #5 on: March 14, 2014, 08:20:31 AM »
Hi John

Not sure these are pure enough, but they're well characterised.

Richard
"Stay out of the black and in the red...there's nothing in this game for two in a bed." - Albert Einstein

John Donovan

  • Administrator
  • Emeritus
  • *****
  • Posts: 3322
  • Other duties as assigned...
    • Probe Software
Re: Ultra Pure TiO2?
« Reply #6 on: March 14, 2014, 10:35:32 AM »
Tim Hopkins pops in here to use our SEM occasionally. I think he is now on his second retirement. He seems to spend most of his time in the Alps and just makes up a few standard blocks now and again to help fund his playboy lifestyle. He's got the right idea!

A casual search of the Internet does not show them, do you have contact info or a web site?
john

Edit by GSeward:
http://www.pandhdevelopments.com/
« Last Edit: October 03, 2014, 05:42:00 PM by Gseward »
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

Malcolm Roberts

  • Professor
  • ****
  • Posts: 134
Re: Ultra Pure TiO2?
« Reply #7 on: May 20, 2014, 11:31:31 PM »
Yes....He's been at that for a number of years now. Always used to brag about living from the wife's old people's home in Glossop or somewhere like that out there. I see it's been all change at Manchester, but I have asked one of my old colleagues if they know of Dave Plant's whereabouts. See what happens......
I could use doing a bit of standard updating here too......
Cheers,
malc.