If you experience any difficulties getting a beam current measurement in Probe Image with your JEOL instrument, there is a place where one can specify a longer delay before the application tries to actually read the beam current *after* inserting the faraday cup. This mainly applies to the newest 8230/850 instruments.
For some reason each new model of JEOL EPMA instrument requires a longer "settling time" after the cup is inserted and before a beam current reading is made.
This is under Setup | Probe Image Setup menu under the Probe Specific Settings dialog as seen here:
![](https://probesoftware.com/smf/oldpics/i61.tinypic.com/2i96z2g.jpg)