Hi All,
This is more of an SEM questions, rather than an EPMA question, but I'm hoping the hivemind can help out...
I have a user who wants to look at magnetic powder particles, and he is asking the best way to prepare these. We've had users sprinkle powders on carbon tape before, but I'm concerned about the magnetic aspect of this material. We don't know the grain size - that's one of the things he wants to determine in the SEM.
Has anybody got any tips and tricks for mounting up magnetic powders for imaging?
Many thanks,
Em