General question about cathodoluminescent (CL) materials. Has anybody got a good CL-specific review article that cites direct comparisons of three prep methods—fluxed growth, hydrothermal growth and crystallization from melt (Verneuil or Czochralski)? And then there are the practical details.
The worst issue with fluxed growth is getting ALL the flux off the crystals. This means some furnace modification to safely invert the crucible at growth temperature, plus reheating the crystals on a mesh to melt off more flux, and finally boiling off the residue. Very long and might not be good enough for CL.
Both former and current commercial production of single crystals use the Verneuil or Czochralski method with no flux (no cleanup). The second advantage of melt growth is that the orientation is well defined for a large area. For some materials including SrTiO3, control of the atmosphere is also essential (see Wikipedia article).
Melt growth is best done on a commercial scale but the price for materials without doping is reasonable. One modification is called micro-pulldown which requires smaller furnace setup. The only limitation is the requirement that no phase transitions occur during cooling (growing many fluorides would not work).
This link is one current source with comprehensive details (although they misspell Verneuil)
https://www.crystalsubstrates.com/en-ca/products/strontium-titanate-srtio3-substratesTheir price for small cuts is low enough to just get a set and start testing. Ask them for a price quote for thicker slices or even an uncut boule (50-100g of consistent material) which would be a one-time purchase.
And for benitoite, old natural specimens had a blue (trace Fe) phase next to a colourless phase which might still be BaTiSi3O9. I have scraps, ~20 grams, if you want to do the workup.